Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0650 GPa | 9.43 ksi | |
LyondellBasell Lupolen® V 3510 K Ethylene Vinyl Acetate, lnjection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.0650 GPa | 9.43 ksi | |
LyondellBasell Lupolen® V 3520 K Ethylene Vinyl Acetate Films, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.0650 GPa | 9.43 ksi | 1 mm/min; ASTM D638 - ISO 527-2 |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Tensile Modulus | >= 0.0650 GPa | >= 9.43 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Modulus | 0.0650 GPa | 9.43 ksi | ISO 527-1/-2 |
DSM Arnitel® EB464-01 TPC-ET Antisqueak Blow Molding Grade |
|||
Tensile Modulus | 0.0650 GPa | 9.43 ksi | 1 mm/min |
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |