Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0200 GPa | 2.90 ksi | ASTM D882 |
DuPont™ Sclairfilm® MPP-1 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Tensile Modulus | 0.0200 GPa | 2.90 ksi | ASTM D882 |
DuPont™ Sclairfilm® MPP-3 LLDPE Film, "Super Strength", 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.An oriented linear low density polyethylene (LLDPE) sealant film that combines exceptional strength and flex-crack characteristics with the outstanding hea.. |
|||
Tensile Modulus | 0.0200 GPa | 2.90 ksi | |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Tensile Modulus | 0.0200 GPa | 2.90 ksi | |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Tensile Modulus | 0.0200 GPa | 2.90 ksi | ISO 527 |
Lubrizol ESTANE® 58214 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |