Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00500 GPa | 0.725 ksi | Young's; ISO 527-3 |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Tensile Modulus | 0.00500 GPa | 0.725 ksi | Young's; ISO 527-3 |
Lushan EV1050G2 EVA Film for Encapsulating Solar modules, High Transmittance EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemical Ac.. |