Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.1 MPa
14200 psi
23°C; 50% RH; ASTM D638
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCON PO6063 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, Electrostatic Dissipation, High Strength, Low WarpageApplication: LCD Cell TrayCAS No. 35134-01-4, 65997-17-3, 7440-44-0 and 7782-42-5Information prov..
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose
Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled
MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled
Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® EM-8240C MPPE, Glass Filled
MPPE/GF material that is used in the main frame of banknote sortersInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled
Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
ASTM D638
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced
Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor..
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 98.1 MPa
14200 psi
ASTM D638
Cheng Yu Plastic ML3420 PC, 20% Glass Fiber
Tensile Strength, Yield 98.1 MPa
14200 psi
ASTM D638
Cheng Yu Plastic NG1100S Nylon 66, 10% Glass Fiber Reinforced
Tensile Strength, Yield 98.1 MPa
14200 psi
ASTM D638
Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber
Tensile Strength, Yield 98.1 - 216 MPa
14200 - 31300 psi
Average value: 145 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Tensile Strength, Yield 98.1 MPa

@Thickness 3.20 mm
14200 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUCON CP6067 PC+CNT+CF
Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74..