Polymer Property : Tensile Strength, Yield = 93.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled  (discontinued **)
Improved Surface. Property data for dry as molded samples.Data provided by the manufacturer
Tensile Strength, Yield 93.0 MPa
13500 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC
LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific)
20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12
LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12
LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri..
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific)
Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D 638
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS
LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA..
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D 638
SABIC Innovative Plastics LNP Thermocomp OF004AER PPS (Asia Pacific)
LNP* Thermocomp* OF004AER is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SA..
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No..
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced
Information provided by Entec
Tensile Strength, Yield 93.0 MPa
13500 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food ..
Tensile Strength, Yield 93.0 MPa
13500 psi
5 mm/min; ISO 527
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta..
Tensile Strength, Yield 93.0 MPa
13500 psi
5 mm/min; ISO 527
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Tensile Strength, Yield 93.0 MPa

@Temperature -40.0 °C
13500 psi

@Temperature -40.0 °F
ISO Data
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced
High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer
Tensile Strength, Yield 93.0 MPa
13500 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength, Yield 93.0 MPa
13500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength, Yield 93.0 MPa
13500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..