Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 9200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.4 MPa
9200 psi
2 in per min; ASTM D638
Network Polymers MS 300 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hylex® P1025FRVNH Polycarbonate
Available in North America Features: Flame Retardant, Halogen Free and High Flow RoHS Compliant Form: PelletsInformation provided by Ravago
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA)
Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS FR 6209
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM 638
PlastxWorld CEVIAN® SKG10 10% GF ABS
Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
Tensile Strength, Yield 63.4 MPa

@Thickness 3.18 mm
9200 psi

@Thickness 0.125 in
6 mm/min; ASTM D638
Chi Mei Acryrex® CM-211 PMMA
Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Asahi Kasei Thermylene® P-15FG-0860 15% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Techmer ES Luriblend® POM CO GF5 TL5 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Composites, In..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 63.4 - 119 MPa

@Temperature 100 - 175 °C
9200 - 17300 psi

@Temperature 212 - 347 °F
Average value: 87.2 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Tensile Strength, Yield 63.4 MPa
9200 psi
ASTM D638
GEHR Plastics Noryl PPO  (discontinued **)
PPO belongs to the group of the amorphous materials and can be used in temperatures ranging from -58 °F to +302 °F. PPO exhibits a high impact strength and a very high dimensional stability. The e..
Copyright © lookpolymers.com All Rights Reserved