Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC/ABS-FR0 Polycarbonate+ABS, Flame Resistant Add "R" for Added Release, "U" for UV Stabilizer and "EF" for Easy Flow (35.0 g/10min)UL Listing: File No. E213588Information provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC/PBT-1020 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC/PBT-1430U Polycarbonate+PBT, Superior Weatherability, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1406 Polycarbonate, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1406FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1418 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1425 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1428 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 62.07 MPa | 9003 psi | ASTM D638 |
Lucent Polymers PC-FR2 Polycarbonate, Flame Resistant Melt Flow Adjustable for ApplicationUL File Number: E213588Add "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |