Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.17 MPa | 1330 psi | ASTM D412 |
Polymax® Maxelast® A9870 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 9.17 MPa | 1330 psi | 200% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 days |
Teknor Apex Flexalloy® 9800-40 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Tensile Strength, Yield | 9.17 MPa | 1330 psi | |
Dow LDPE 4012M Low Density Polyethylene DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge.. |