Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D412 |
Polymax® Maxelast® A9950C TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D638 |
Global ST-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D638 |
Global SU-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | @100% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 605 Perfluoroelastomer Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and e.. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D 638 |
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces.. |
|||
Tensile Strength, Yield | 9.03 MPa | 1310 psi | ASTM D638 |
Global S-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |