Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.1 - 59.3 MPa @Temperature -18.0 - 71.0 °C |
3210 - 8600 psi @Temperature -0.400 - 160 °F |
Average value: 40.7 MPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |