Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.156 MPa
1183 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 2870 Thermoplastic Elastomer
Elastocon® 2870 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2870 is FDA compliant and well suited for cons..