Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 550 MPa | 79800 psi | |
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 550 - 760 MPa | 79800 - 110000 psi | |
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 550 - 760 MPa | 79800 - 110000 psi | |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | >= 550 MPa | >= 79800 psi | |
MetalTek MTEK CA6NM Cast UNS J91540 Martensitic Stainless Steel "400" series, General corrosion resistant alloys, high strength.Applications: Chemical and food process equipment, jet engine compressor cases and rocket engine parts.Information provided by MetalTe.. |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 % |
79800 psi @Strain 0.200 % |
|
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 %, Temperature 650 °C |
79800 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 25 alloy, cold worked sheet, 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 % |
79800 psi @Strain 0.200 % |
|
Haynes 556® alloy, 40% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 550 MPa | 79800 psi | Annealed |
Special Metals INCOLOY® Alloy MA 956 An iron-chromium-aluminum alloy that is oxide dispersion strengthened and produced by mechanical alloying. Production involves high-energy milling of metal powders to create an alloy with a strengt.. |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 % |
79800 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 263 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an.. |
|||
Tensile Strength, Yield | >= 550 MPa | >= 79800 psi | After bake hardening |
SSAB Tunnplat Docol® 800 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 % |
79800 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v.. |
|||
Tensile Strength, Yield | >= 550 MPa | >= 79800 psi | |
ThyssenKrupp PAS 550 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Tensile Strength, Yield | 550 MPa | 79800 psi | |
ThyssenKrupp SECURE 200 Structural Steel This Material Specification applies to heavy plates from 3 to 15 mm in thickness made of the high-strength armour steel SECURE 200 (ThyssenKrupp armour steel) with a minimum hardness of 200 HBW and .. |
|||
Tensile Strength, Yield | 550 - 750 MPa @Strain 0.200 % |
79800 - 109000 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Yield | >= 550 MPa | >= 79800 psi | |
AK Steel Full Hard Only, Grade 80 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 550 MPa @Strain 0.200 % |
79800 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 4 Titanium (UNS R50700) Uses: CPI equipment, industrial components, heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 550 - 650 MPa | 79800 - 94300 psi | |
ArcelorMittal HSLA 550 High strength low alloy steel for cold forming, Hot Rolled Available in the following: S550MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w.. |
|||
Tensile Strength, Yield | 550 MPa | 79800 psi | |
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Tensile Strength, Yield | 550 MPa | 79800 psi | |
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
Tensile Strength, Yield | >= 550 MPa @Strain 0.200 % |
>= 79800 psi @Strain 0.200 % |
|
Schmolz + Bickenbach UGICHROM 244 Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coeffici.. |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |
|||
Tensile Strength, Yield | 550 - 690 MPa | 79800 - 100000 psi | |
Materion Beryllium Copper Alloy 3 Tube; AT (TF00) Temper; All Sizes (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |