Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T.. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF10 L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES Plastiblend® TPX-HTN-000AA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength, Yield | 77.9 MPa | 11300 psi | ASTM D638 |
PlastxWorld Veroplas PB2009L Nylon 66 general purpose, unfilled, lubricated injection molding gradeInformation provided by PlastxWorld Inc. |