Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | ASTM D882 |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | ASTM Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 49.6 MPa | 7190 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ASAPC 122954H Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |