Polymer Property : Tensile Strength, Yield = 7020 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.4 - 58.0 MPa
7020 - 8410 psi
Average value: 53.5 MPa Grade Count:15
Overview of materials for Chlorinated PVC (CPVC)
This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Yield 48.4 MPa
7020 psi
ASTM D638
Westlake Plastics Corzan® II CPVC Sheet
Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual..