Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.80 MPa

@Strain 50.0 %
1130 psi

@Strain 50.0 %
50 mm/min
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..