Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 68.9 MPa | 9990 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ DC-818.G001-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Omni Plastics OmniTech™ HDPE GRC30 Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | >= 68.9 MPa | >= 10000 psi | Clear Casting |
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Tensile Strength, Yield | 68.9 - 150 MPa | 10000 - 21800 psi | Average value: 106 MPa Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | ASTM D882 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled
(discontinued **) PRELIMINARY DATA SHEETDescription/Features:Glass Fiber ReinforcedBlackInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Fiberfil® J-60/20/E4 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® HIPS GF30 30% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GB15 L BK 15% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 15% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Good UV Resistance and LubricatedAppearance: BlackTPCI# .. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES HiFill® PEEK HF Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 LX Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 IM 3757 Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM 638 |
PlastxWorld CEVIAN® SERG1 10% GF ABS Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Ensinger Tecamid® HS Nylon (PA) Heat Stabilized nylon, increased ability to withstand the negative effects of heat exposure and increased overall service temperature over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 9990 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers SAN 330 BEADS Styrene Acrylonitrile, Transparent Engineering Thermoplastic, High Flow Natural Beads Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-1740 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-2153 20% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-1734 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 68.9 MPa | 10000 psi | ASTM 638 |
PlastxWorld CEVIAN® SUG20 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |