Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 448 MPa | 65000 psi | |
Pacific Sintered Materials FCC-216-P(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Tensile Strength, Yield | 448 MPa @Temperature 71.1 °C |
65000 psi @Temperature 160 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 448 MPa @Temperature 21.1 °C |
65000 psi @Temperature 70.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, Spectra® 951 - PT Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 448 MPa @Temperature 23.9 °C |
65000 psi @Temperature 75.0 °F |
ASTM D3039 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Tensile Strength, Yield | >= 448 MPa | >= 65000 psi | |
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Tensile Strength, Yield | 448 MPa | 65000 psi | |
Kennametal Stellite Hydroloy® HQ913® Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Proprietary stainless steel with low Co and Mn contents, formulated to resist cavitation and dro.. |
|||
Tensile Strength, Yield | >= 448 MPa | >= 65000 psi | |
Kinetics MIM F75 (ASTM F75) HIP Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Tensile Strength, Yield | 448 - 517 MPa @Strain 0.200 % |
65000 - 75000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 448 - 517 MPa @Strain 0.200 % |
65000 - 75000 psi @Strain 0.200 % |
|
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 448 - 862 MPa | 65000 - 125000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Yield | 448 - 586 MPa @Strain 0.200 %, Thickness >=25.4 mm |
65000 - 85000 psi @Strain 0.200 %, Thickness >=1.00 in |
Turned Bars |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Tensile Strength, Yield | 448 MPa @Strain 0.200 % |
65000 psi @Strain 0.200 % |
|
Universal Wire Works 321 Stainless Steel (AMS 5689) Filler Metal Universal 321 is a titanium-stabilized filler metal used with the gas metal arc and gas tungsten arc processes. Universal 321 stabilized weldments are often subjected to severe corrosive and high te.. |
|||
Tensile Strength, Yield | 448 - 490 MPa | 65000 - 71000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 448 - 490 MPa | 65000 - 71000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, Extra Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 448 - 496 MPa | 65000 - 72000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, Extra Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | 448 - 510 MPa | 65000 - 74000 psi | 0.2% offset |
Eagle Brass 240 Low Brass, Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Yield | >= 448 MPa | >= 65000 psi | 0.2% offset |
Eagle Brass 7026 Copper Nickel, Annealed 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 448 MPa | >= 65000 psi | 0.2% offset |
Eagle Brass 70265 XP175, Annealed Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 448 MPa | 65000 psi | |
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
Tensile Strength, Yield | 448 MPa | 65000 psi | Hard |
California Fine Wire Copper Clad 1006 Steel (40% Conductivity) All values may vary dependent on specific design and usage1006 steel core, 99.99% copper cladCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | >= 448 MPa @Strain 0.200 % |
>= 65000 psi @Strain 0.200 % |
|
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Tensile Strength, Yield | >= 448 MPa @Strain 0.200 % |
>= 65000 psi @Strain 0.200 % |
|
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Tensile Strength, Yield | 448 - 586 MPa @Strain 0.200 % |
65000 - 85000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 448 - 586 MPa @Strain 0.200 % |
65000 - 85000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 448 MPa | 65000 psi | Typical |
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy Ohmaloy 40 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |
|||
Tensile Strength, Yield | 448 - 586 MPa @Strain 0.200 % |
65000 - 85000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 448 MPa @Strain 0.200 % |
65000 psi @Strain 0.200 % |
|
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Tensile Strength, Yield | 448 MPa @Strain 0.200 %, Temperature -73.0 °C |
65000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |