Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 64.8 MPa | 9400 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/10T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | chs 2 in/min; ASTM D638 |
Network Polymers PC-1006 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | chs 2 in/min; ASTM D638 |
Network Polymers PC-1006 L Description: Colors and Natural Polycarbonate with UVInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | chs 2 in/min; ASTM D638 |
Network Polymers PC-1010 Description: Polycarbonate, 10% Glass Filled BlackInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 64.8 MPa @Thickness 3.17 mm |
9400 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 64.8 - 146 MPa | 9400 - 21200 psi | Average value: 94.6 MPa Grade Count:7 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Yield | 64.8 MPa @Temperature 22.8 °C |
9400 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Sintimid™ V 40% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Tensile Strength, Yield | 64.8 MPa @Thickness 3.17 mm |
9400 psi @Thickness 0.125 in |
Injection Molded; ASTM D638 |
Global 100-25 LDPE Polyethylene Commercial-grade, low-density polyethylene with good dimensional stability, toughness and softness.Good dimensional stabilitySoftGood toughnessApplications:CapsClosures |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Global GPC-110 10% Glass Reinforced Polycarbonate Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Spartech Polycast SP 1.25 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Techmer ES Luriblend® PA6/12 01430 Nylon 612 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ASA FR1508 UV Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 64.8 MPa @Thickness 3.20 mm |
9400 psi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron XU 73120.00 Polycarbonate Resin Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Techmer ES HiFill® PP CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Westlake Plastics Zelux® CN-P Polycarbonate (conductive) Carbon-powder-filled with high flexural strength and good thermal stability to 275F. The CN-P is UL94 V-0 rated at 0.030" and is thermoformable in thinner gauges (0.010"-0.060").Information provide.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Tensile Strength, Yield | 64.8 MPa | 9400 psi | ASTM D638 |
PlastxWorld Veroplas PA2000 Nylon 6 general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc. |