Polymer Property : Tensile Strength, Yield = 638 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.40 MPa
638 psi
ASTM D412
Polymax® Maxelast® P52-004A-3B TPE, PP Overmold or Standalone use
Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra..
Tensile Strength, Yield 4.40 MPa
638 psi
-20% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S70N Silicone Rubber
Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade ..
Tensile Strength, Yield 4.40 MPa
638 psi
-20% change after 336 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80N Silicone Rubber
Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade ..
Tensile Strength, Yield 4.40 MPa
638 psi
M100
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle..
Tensile Strength, Yield 4.40 MPa
638 psi
M100
3M Dyneon™ Fluorel™ FE-5830Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 70.5%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 70.5% F grade terpolymer with best pe..
Tensile Strength, Yield 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ASTM D638
Toyobo A1080A Thermoplastic Polyurethane Elastomer, Injection Grade
Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,..
Tensile Strength, Yield 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of..
Tensile Strength, Yield 4.40 MPa
638 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-180 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.40 MPa

@Strain 100 %
638 psi

@Strain 100 %
ASTM D638
Toyobo E1080A Thermoplastic Polyurethane Elastomer, Extrusion Grade
Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,..