Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 63.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.8 MPa
9250 psi
ASTM D638
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
Tensile Strength, Yield 63.8 - 167 MPa
9250 - 24200 psi
Average value: 89.5 MPa Grade Count:7
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Tensile Strength, Yield 63.8 MPa
9250 psi
ISO 527-2
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Tensile Strength, Yield 63.8 MPa
9250 psi
ISO 527-2
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA)
Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru..
Copyright © lookpolymers.com All Rights Reserved