Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM D638M |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | |
Ineos ABS Centrex® 821 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM D638 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Strength, Yield | 43.4 MPa @Temperature 23.0 °C |
6290 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene GP150 Polystyrene APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 9015 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | 105% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6290 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS TS-12 Injection Molding Grade, Medium Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |