Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B930 (Base Grade), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B932 (UV Inhibitor Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9304 (Odor Mask Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9324 (UVI, Odor Mask Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 9085 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 9450P ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 42.7 MPa @Thickness 3.17 mm |
6190 psi @Thickness 0.125 in |
|
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 42.7 MPa | 6190 psi | ASTM Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |