Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.20 MPa @Strain 100 % |
609 psi @Strain 100 % |
|
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Tensile Strength, Yield | 4.20 MPa | 609 psi | 50 microns film; ASTM D882 |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Tensile Strength, Yield | 4.20 MPa | 609 psi | 50 microns film; ASTM D882 |
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group |