Polymer Property : Tensile Strength, Yield = 60.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.6 MPa

@Thickness 3.17 mm
8790 psi

@Thickness 0.125 in
ASTM D638
Chi Mei Kibisan® PN107 SAN Resin, General Purpose
Product CharacteristicsWater ClearHigh RigidityMedium FlowInformation provided by Calsak Corporation