Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 60.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
ASTM D638
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 60.3 MPa

@Thickness 3.17 mm
8750 psi

@Thickness 0.125 in
ASTM D638
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Copyright © lookpolymers.com All Rights Reserved