Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.17 MPa | 8002 psi | ASTM D638 |
Lucent Polymers PC/ABS-0406 Polycarbonate+ABS, Injection Grade Recycled ContentAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 55.17 MPa | 8002 psi | ASTM D638 |
Lucent Polymers PC/ABS-1208 Polycarbonate+ABS, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 55.17 MPa | 8002 psi | ASTM D638 |
Lucent Polymers PC/ABS-1216LG Polycarbonate+ABS, Low Gloss, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 55.17 MPa | 8002 psi | ASTM D638 |
Lucent Polymers PC/PET-1515 Polycarbonate+PET, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |