Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | |
Ineos ABS Lustran® LGA Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | 2 in/min; ASTM D638 |
Ineos H12E-00 Polypropylene Homopolymer, Antistatic An antistated polypropylene homopolymer produced by Ineos utilizing catalyst technology.It is designed for injection molding and general purpose extrusion. This material meets the Food and Drug Adm.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | 50mm/min; ISO 527-2 |
Borealis HG385MO Polypropylene HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polyprop.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | 87% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9500P Injection Molding Grade, Ultra High Impact Powder Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | |
Bapolan® ABS8430 ABS Polymer, Extrusion/Injection Grade Applications: Electronic Instruments, appliances.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength, Yield | 36.5 MPa @Thickness 3.20 mm |
5290 psi @Thickness 0.126 in |
51mm/min; ASTM D638 |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |
|||
Tensile Strength, Yield | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |