Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa

@Thickness 3.20 mm
5100 psi

@Thickness 0.126 in
At 51mm/min, thick injection molded ASTM Type 1 specimen; ASTM D638
Pinnacle Polymers 1508 Polypropylene Homopolymer, Fiber Spinning Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Tensile Strength, Yield 35.2 MPa
5100 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH005 Polypropylene, Homopolymer, Extrusion, Strapping
COPYLENE® CH005 is a fractional melt flow polypropylene homopolymer resin available in pellet form.Information provided by Phillips 66.
Tensile Strength, Yield 35.2 MPa
5100 psi
(2 in/min); ASTM D638
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer
COPYLENE™ CH350 is a controlled rheology, barefoot homopolymer designed for application as a base resin for compounding, consumer products and other injection molding applications.Applications: Inj..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D 638
LyondellBasell Moplen HP400L Polypropylene Homopolymer
Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure capsInformation provid..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D 638
LyondellBasell Moplen HP400N Polypropylene Homopolymer
Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D 638
LyondellBasell Moplen HP550J Polypropylene Homopolymer
Description: HP550J, a general purpose polypropylene homopolymer resin, is suitable for general extrusion and film fiber applications. HP550J resin meets FDA requirements in the Code of Federal Reg..
Tensile Strength, Yield 35.2 MPa
5100 psi
2 in/min; ASTM D638
M. Holland Company PP500 Polypropylene Homopolymer
Features: Homopolymer, Narrow Molecular Wt. Dist.Uses: Disposable Drinkware, Medical Applications, PackagingApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by ..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Global ABS-704 General Purpose High Impact ABS
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 35.2 MPa

@Temperature 23.0 °C
5100 psi

@Temperature 73.4 °F
ASTM D638
Ineos H02G-02 Polypropylene Homopolymer
This is a homopolymer designed for extrusion and film. It exhibits good extrusion and film orientation behavior. This material meets the requirements of the U.S. Food and Drug Administration as sp..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Greene Tweed ARâ„¢ HT Abrasive-Resistant Thermoplastic
ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Spartech DP5120 Talc Filled Homopolymer
Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Techmer ES Plastiblend® ABS 7000
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
Tensile Strength, Yield 35.2 MPa
5100 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® 5140N Homopolymer Polypropylene
Homopolymer for Injection Molded Applications Formolene 5140N is a highly isotactic, polypropylene homopolymer with fast cycle time and improved mold release. It has use in injection molded applicat..
Tensile Strength, Yield 35.2 MPa
5100 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS VP-12
Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 35.2 MPa
5100 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA S190
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 35.2 MPa
5100 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 35.2 MPa
5100 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 35.2 MPa
5100 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Dow H110-02N Polypropylene Resin
DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowD..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Amco Amalloy® B1172 Polymer Alloy
Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials.
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Amco PRIMATOP HDPE RP 011 Granular High Density Polyethylene
HDPE RP 011 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013.
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Aaron Industries AAROLENE® ARPP H 200-1 PP Black Polypropylene Homopolymer Compounded Resin
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinFeatures: A pre-colored, black homopolymer polypropylene resin specifically designed for all injection molding applications.High Flow
Tensile Strength, Yield 35.2 MPa
5100 psi
2" (50mm) per min; ASTM D638
Formosa Plastics Formolene® 5181K Homopolymer Polypropylene
Homopolymer for Extrusion Applications Including Straws Formolene® 5181K is a high molecular weight, highly isotactic, polypropylene homopolymer containing anti-stat designed for straws and cutlery..
Tensile Strength, Yield 35.2 MPa

@Temperature 23.0 °C
5100 psi

@Temperature 73.4 °F
ASTM D638
Ineos H12G-00 Polypropylene Homopolymer
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsG..
Tensile Strength, Yield 35.2 MPa
5100 psi
ASTM D638
Techmer ES HiFill® PA12 1100 Tungsten Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc.