Polymer Property : Tensile Strength, Yield = 5.90 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.90 MPa
856 psi
M100
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. ..
Tensile Strength, Yield 5.90 MPa
856 psi
M100
3M Dyneon™ Fluorel II™ FX-11900 Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 59%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Good metal a..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 2005 Carbon Sponge Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
Conductive Layer
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors
Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb..
Tensile Strength, Yield 5.90 MPa
856 psi
100% elongation; ASTM D412
Lubrizol Estane® 5712 Thermoplastic Polyurethane
Type: Estane® 5712 is a Polyester thermoplastic polyurethane (TPU).Feature: It has the highest peel and green strengths and shortest open-tack time of any Estane TPU resin used in adhesives. Suppl..
Tensile Strength, Yield 5.90 MPa
856 psi
Dow AFFINITY™ SM 1300 Polyolefin Plastomer
AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu..
Tensile Strength, Yield 5.90 MPa
856 psi
508 mm/min; ASTM D638
Dow Engage® 8440 Polyolefin Elastomer
Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer ..
Tensile Strength, Yield 5.90 MPa

@Strain 50.0 %
856 psi

@Strain 50.0 %
50 mm/min
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema.
Tensile Strength, Yield 5.90 MPa

@Strain 100 %
856 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.