Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.7 MPa | 4890 psi | ISO 527-2/5 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Tensile Strength, Yield | 33.7 MPa | 4890 psi | 80% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 33.7 MPa | 4890 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ HMU 210 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness for automotive HVAC and under-the-hood applications.Availability: Africa & Middle East, Asia Pacif.. |