Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.6 MPa
7050 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging M2288 Polyvinyl Chloride, Rigid (PVC, Rigid)
Opaque sheet extrusion compound.Information provided by PolyOne
Tensile Strength, Yield 48.6 MPa
7050 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Dry Blend E1354 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 48.6 MPa
7050 psi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 48.6 MPa
7050 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SRF 1807 Polyvinyl Chloride, Rigid
Availability: Asia Pacific Features: Good Flow; Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Copyright © lookpolymers.com All Rights Reserved