Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.5 MPa | 7030 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Amber 9360 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.5 MPa | 7030 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Amber 9375 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.5 MPa | 7030 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Polyvinyl Chloride, Rigid (PVC, Rigid) This product is available in opaque and transparent colors.Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.5 MPa | 7040 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBB 3700 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |