Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.2 MPa | 4090 psi | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Tensile Strength, Yield | 28.2 MPa | 4090 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® M5350 High Density Polyethylene ApplicationsALATHON M 5350 copolymer with narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing s.. |
|||
Tensile Strength, Yield | 28.2 MPa | 4090 psi | ISO 527-2/50 |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Tensile Strength, Yield | 28.2 MPa | 4090 psi | 20 in/min; CP-TM-09 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |