Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.04 MPa
586 psi
200%, post cured- 8 hours at 177°C
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.04 MPa
586 psi
chs 20 in/min; 300% elongation; ASTM D412
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.