Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.7 MPa | 3870 psi | 64% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength, Yield | 26.7 MPa | 3870 psi | ASTM D638 |
Entec Hypro™ PPC-T30 Copolymer Polypropylene, 30% Talc Reinforced Information provided by Entec |