Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.5 MPa | 3850 psi | ASTM D638 |
Multibase Multi-Pro® 5014 CUW Polypropylene Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss a.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | ASTM D638 |
M. Holland Company CP100 Polypropylene Impact Copolymer Impact copolymerHigh impact resistanceLow temperature impact resistanceApplications: PipingSheetInformation provided by M. Holland |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | ASTM D638 |
M. Holland Company CP420 Polypropylene Impact Copolymer AntistaticImpact copolymerGood impact resistanceLow temperature impact resistanceNucleatedApplications: Fishing applicationsFurnitureTool/tote box |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |