Polymer Property : Tensile Strength, Yield = 37.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.6 MPa
5450 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Tensile Strength, Yield 37.6 MPa
5450 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH120LN Polypropylene, Homopolymer, Injection Molding, Antistat/Lube
COPYLENE™ CH120LN is designed for general purpose injection molding applications with anti-static and nucleation. Applications: Food Containers, Housewares, Closures.Information provided by Phillip..
Tensile Strength, Yield 37.6 MPa
5450 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH350LN Polypropylene, Homopolymer, High Flow, Nucleated, Lube, Injection Molding
COPYLENE™ CH350LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio..
Tensile Strength, Yield 37.6 MPa
5450 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH200LN Polypropylene, Homopolymer, CR, Antistat, Nucleated, Injection Molding
COPYLENE™ CH200LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio..
Tensile Strength, Yield 37.6 MPa
5450 psi
ASTM D638
Spartech Royalite R59M Hi-Impact ABS/PVC Resin
Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t..
Tensile Strength, Yield 37.6 MPa
5450 psi
50 mm/min; ASTM D638
Amco PRIMATOP PP HOMO 120 Injection Molding Polypropylene
Features:medium viscosityexcellent processabilitygood stiffnessenvironmental stress crack resistanceheat performanceminimal odor and tasteApplications:closuressmall applianceshousewarestoyscontains ..