Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 290 - 365 MPa | 42000 - 53000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, 1/2 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Yield | 172 - 365 MPa | 25000 - 53000 psi | |
Chicago Extruded Metals UNS C48200 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 172 - 365 MPa | 25000 - 53000 psi | |
Chicago Extruded Metals UNS C48500 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |