Mechanical Properties Metric English Comments
Tensile Strength, Yield 239 MPa
34700 psi
ISO 527-2
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..