Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.39 MPa | 3393 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-95 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 23.39 MPa | 3393 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 23.39 MPa | 3393 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 23.39 MPa | 3393 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-95 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |