Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.31 MPa | 335 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | >= 2.31 MPa | >= 335 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 38-113 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalUV StabilizedApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First Cho.. |
|||
Tensile Strength, Yield | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3840MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentUV StabilizedApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tensile Strength, Yield | 2.31 MPa @Strain 300 % |
335 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® ST-6140 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs.. |