Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.3 MPa | 3240 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 22.3 MPa | 3240 psi | ASTM D638 |
Entec Hypel® PEHD8/.955 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 22.3 MPa | 3240 psi | ASTM D 638 |
Styrolution PS 5600/5601 HIPS Fine balance of toughness and rigidityGood processabilityUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 22.3 MPa | 3240 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |