Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers
Tensile Strength, Yield 22.1 - 59.3 MPa

@Temperature -18.0 - 71.0 °C
3210 - 8600 psi

@Temperature -0.400 - 160 °F
Average value: 40.7 MPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Tensile Strength, Yield 22.1 MPa
3210 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 18% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 18% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Tensile Strength, Yield 22.1 MPa
3210 psi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite 380A3V32818 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D638
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM Data
Dow AIM® 4900 High Impact Styrenic Resin
AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss..
Tensile Strength, Yield 22.1 MPa
3210 psi
Molded property
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..
Tensile Strength, Yield 22.1 MPa
3210 psi
Dow HDPE 30460M High Density Polyethylene
DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro..
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D-638
Axiall 15642 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
Tensile Strength, Yield 22.1 MPa
3210 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Tensile Strength, Yield 22.1 MPa
3210 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Tensile Strength, Yield 22.1 - 41.4 MPa
3210 - 6000 psi
Average value: 30.5 MPa Grade Count:74
Overview of materials for Cellulose Acetate Propionate, Molded