Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.5 MPa | 4710 psi | ASTM D638 |
IRPC Polimaxx Polene GM2865 High Density Polyethylene CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL.. |
|||
Tensile Strength, Yield | 32.5 MPa | 4710 psi | ISO 527-2 |
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w.. |
|||
Tensile Strength, Yield | 32.5 MPa | 4710 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 32.5 MPa | 4710 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |