Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 3120 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.5 MPa
3120 psi
2 in per min; ASTM D638
Network Polymers NPP 25-0414
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 21.5 MPa
3120 psi
2 in per min; ASTM D638
Network Polymers NPP 25-0616
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 21.5 MPa
3120 psi
2 in per min; ASTM D638
Network Polymers NPP 25-061601
Description: Impact Modified PolypropyleneInformation provided by Network Polymers Inc.
Tensile Strength, Yield 21.5 MPa
3120 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers SEQUEL® 1402 TPO  (discontinued **)
Description: SEQUEL® 1402 engineered polyolefin material is designed for large automotive exterior applications that require high melt flow, excellent paintability, and processability. Applications..
Tensile Strength, Yield 21.5 MPa
3120 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers SEQUEL® 1493 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1493 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent p..
Tensile Strength, Yield 21.5 MPa
3120 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact propertie..
Tensile Strength, Yield 21.5 MPa
3120 psi
ASTM D638
Tipco Tipcolene® FPZ-CL - 10% Talc/Mineral Reinforced Polypropylene Copolymer Compound
10% Mineral Reinforced PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Yield 21.5 MPa
3120 psi
ASTM D638
Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow
20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Yield 21.5 MPa
3120 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers NPP25-0616 Black Impact Modified Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 21.5 MPa
3120 psi
50 mm/min
Arkema Group Appryl® 3130 MU 7 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive industry. It ..
Tensile Strength, Yield 21.5 MPa
3120 psi
Radici Radilene® R 70 IE 5058 B High Density Polyethylene
Shore hardness: 64 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a..
Copyright © lookpolymers.com All Rights Reserved