Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.03 MPa | 440 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.03 MPa | 440 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.03 MPa | 439 psi | ASTM D412 |
Polymax® Maxelast® P3932C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 3.03 MPa | 440 psi | at 200%, molded-without post cure; ASTM D412 |
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |