Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.9 MPa | 4190 psi | ASTM D638 |
Petromont 3101 High Density Polyethylene Resin Petromont HDPE 3101 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for a broad range of injection moulding applications including open-head pails, h.. |
|||
Tensile Strength, Yield | 28.9 MPa | 4200 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger.. |
|||
Tensile Strength, Yield | 28.9 MPa | 4200 psi | |
Zylog Hipolyene® 9221 XM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |