Polymer Property : Tensile Strength, Yield = 27000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide
30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.
Tensile Strength, Yield 186 MPa

@Strain 0.200 %,
Temperature 760 °C
27000 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 186 MPa
27000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Tensile Strength, Yield 186 MPa
27000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6 GF33 HS L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Heat Stabilized, Good UV..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6/10 GF50 L 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF33 HR L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated and Hydrolysis Resistant TPCI# 9357101Informatio..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Luriblend® PA6/6 CF20 TS15 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(10%) and Silicone Lubricant Features: Lubricated, Good Wear Resistance and L..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Luriblend® PA6/6 CF30 TS15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Silicone LubricantFeatures: Lubricated, Low Friction and Good Wear ..
Tensile Strength, Yield 186 MPa
27000 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UFW49RS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UFW49RS is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 186 MPa
27000 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UFW49RSC PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UFW49RSC is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features include: Heat Stabilized.
Tensile Strength, Yield 186 MPa
27000 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Tensile Strength, Yield 186 MPa
27000 psi
Type I, 5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES HiFill FR® PA6 GF/M50 FR 50% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Tensile Strength, Yield 186 MPa
27000 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX99732C PA 66
LNP* Thermocomp* PDX-R-99732 is a Nylon 6/6 with proprietary fillers.
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..
Tensile Strength, Yield 186 MPa

@Temperature 22.8 °C
27000 psi

@Temperature 73.0 °F
ASTM D638
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow
Data provided by Clariant Masterbatches
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Clariant Renol PA111G33 Nylon 66, 33% Glass Fiber
Data provided by Clariant Masterbatches
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 186 MPa

@Strain 0.200 %
27000 psi

@Strain 0.200 %
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy
Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems.Property values are for samples in the metallurgical condition: 2100°..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Luriblend® HTN 01400 BK
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, ..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric..
Tensile Strength, Yield 186 MPa
27000 psi
ASTM D638
Techmer ES Electrablend® PA6 E CF20 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Conductive Appearance: Natural ColorProcessing Method: ExtrusionInformation p..