Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
NYCOA 27/330KNF Glass Filled Nylon 6 33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | |
Pacific Sintered Materials FC-203-N Copper Iron Powdered Metal Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-1000-20All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | |
Pacific Sintered Materials FC-208-N Copper Iron Powdered Metal Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-2000-K40All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 179 MPa @Temperature 23.9 °C |
26000 psi @Temperature 75.0 °F |
0° Direction, Dry; 8HS form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | |
PSM Industries Pacific Sintered Metals Copper Iron FC-208-N Powdered Metal Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-2000-K40Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | |
Kinetics MIM 316 Stainless Steel (Premium Grade) Austenitic stainless steel. Excellent corrosion resistance. Excellent elongation. Non-magnetic. Easily weldable. Can be polished to a mirror finish. Provides better elongation and ductility over the.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 CF20 L 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Semi Conductive and LubricatedInformation provided by TP C.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 CF20 L BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInfo.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6,6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricatedFeatures: LubricatedProcessing Method: Injection MoldingAppearance: .. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 CF20 TL15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance:.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 179 - 441 MPa | 26000 - 64000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, 1/4 Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 179 - 269 MPa | 26000 - 39000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), 1/4 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | ASTM D638 |
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 179 - 269 MPa | 26000 - 39000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), 1/4 Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | 179 MPa @Strain 0.200 %, Temperature 760 °C |
26000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | |
AK Steel Cold Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Tensile Strength, Yield | 179 MPa @Strain 0.200 %, Temperature 927 °C |
26000 psi @Strain 0.200 %, Temperature 1700 °F |
|
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Tensile Strength, Yield | 179 MPa | 26000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |